Abstract

Carpenter titanium alloy Ti 6Al-4V ELI is a high-purity (extra-low-interstitial) version of Ti 6Al-4V (see Alloy Digest Ti-60, August 2002). The alloy is alpha plus beta and has good biocompatibility. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive, shear, and bearing strength as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: TI-129. Producer or source: Carpenter Technology Corporation.