Abstract

Crucible A-286 is an age-hardenable austenitic Fe-Ni-Cr alloy designed for service up to 704 deg C (1300 deg F) on jobs requiring high strength and good corrosion resistance at the operating temperature. The alloy offers high ductility in notched sections. Crucible A-286 is used in jet engines and superchargers for various high-temperature components and is one of the few age-hardenable alloys used for bolting in the ASME Boiler and Pressure Vessel Code. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-851. Producer or source: Crucible Specialty Metals.

This content is only available as a PDF.