Abstract
Incomag Alloy 4 is a direct-melt addition alloy for the production of ductile iron. The addition of this alloy improves the efficient transfer of magnesium to the melt with resulting high recoveries of magnesium. This datasheet provides information on composition and physical properties. Filing Code: Ni-580. Producer or source: International Nickel Inc.