Wieland-N37 is a leaded nickel silver with excellent machining properties. It is available either as an extruded or drawn product. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, and joining. Filing Code: CU-678. Producer or source: Wieland Metals Inc., Wieland-Werke AG.