Abstract
Wieland-N31 is a leaded nickel silver with excellent machining properties. It is suitable for manufacturing a wide variety of sections and precision turned and hot stamped parts requiring higher mechanical strength and higher corrosion resistance than that for brass. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: CU-676. Producer or source: Wieland Metals Inc., Wieland-Werke AG.