Abstract

Wieland-M05 is copper-zinc bronze alloy with good conductivity and beautiful red color. The color allows the alloy to be used in decorative applications. The alloy has also been called gilding metal 95%, and CA 210. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CU-690. Producer or source: Wieland Metals Inc., Wieland-Werke AG.