Abstract

Allegheny Ludlum Type 305 (S30500) stainless steel is used for applications requiring a low rate of work hardening during severe cold-forming operations such as deep drawing. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as heat treating and joining. Filing Code: SS-840. Producer or source: Allegheny Ludlum Corporation.