Abstract

Ti-6Al-2Sn-2Zr-2Mo-0.05Si alloy is used as heavy section forgings that require high strength, fracture toughness, and high modulus. It is used as forgings and sheet for air frames. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and bend strength as well as fracture toughness and creep. It also includes information on high temperature performance as well as joining. Filing Code: TI-119. Producer or source: RMI Company.