ALZ 409 is a ferritic stainless steel with approximately 11% chromium. It has an oxidation and corrosion resistance that is much better than that of mild steel. ALZ 409 has a good combination of formability and weldability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. Filing Code: SS-827. Producer or source: ALZ nv.