Kubota KHR45A LC is a modification of KHR45A (Alloy Digest Ni-570, July 2001) that changes either ductility or carburization resistance. The typical application is as outlet tubes and fittings in pyrolysis service. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance, and corrosion resistance. Filing Code: Ni-571. Producer or source: Kubota Metal Corporation.