Abstract

Märker/Centralloy H101 is a Fe-Ni-Cr alloy matrix, designed to combine adequate strength with structural stability. Although originally designed to be a centrispun cast alloy, it is now available in static and investment cast product forms. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on machining and joining. Filing Code: Ni-569. Producer or source: Schmidt & Clemens Inc.