Abstract
Lescalloy Jethete M-152 ESR is a martensitic stainless steel that is hardenable to product high strength for structural components. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, and joining. Filing Code: SS-818. Producer or source: Timken Latrobe Steel.