Abstract

Avesta Polarit 430 Ti is a ferritic stainless steel with good high-temperature strength and an optimal weldability and formability. The alloy is not susceptible to chloride-ion stress-corrosion cracking, has good resistance to oxidation, and very good aqueous corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming and joining. Filing Code: SS-837. Producer or source: AvestaPolarit AB.