Abstract

Sandvik 7RE10 is a 25Cr/20Ni oxidation-resistant alloy with good carburization and oxidation resistance. It is typically used as furnace tubing. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-812. Producer or source: Sandvik.