Abstract

AUR-O-MET 57 is a high nickel-aluminum bronze that was developed primarily for its abrasion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on heat treating, machining, and joining. Filing Code: Cu-42. Producer or source: Aurora Metal Company.

This content is only available as a PDF.