Abstract
YELLOW BRASS is a copper-zinc alloy having excellent cold working properties with good corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on forming, heat treating, machining, and joining. Filing Code: Cu-41. Producer or source: Brass mills.