Abstract

NITRALLOY N is a special alloy steel which can be nitrided, that is, surface hardened, without final quenching, by the action of ammonia gas at relatively low temperatures. The presence of an appreciable amount of nickel in Nitralloy N both strengthens and toughens the case and develops dispersion hardening in rhe core during nitriding. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-39. Producer or source: Alloy steel mills and foundries.