Abstract

X-ITE is a high chromium-nickel casting alloy having high resistance to corrosion, heat and abrasion. It corresponds to A.C.I. Type HU alloy. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: SS-40. Producer or source: General Alloys Company.