Abstract
JALCASE No. 4 is a low-carbon, free machining case-hardening steel, equivalent to AISI C-1117. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on heat treating and machining. Filing Code: CS-5. Producer or source: Jones & Laughlin Steel Corporation.