Boehler K340 ISODUR has a balanced composition for cold work forming operations like stamping and cutting. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on high temperature performance as well as heat treating and machining. Filing Code: TS-580. Producer or source: Böhler.