Abstract
Alcoa alloy 2090-T83 is an aluminum-lithium sheet alloy with a combination of strength, low density, and corrosion resistance. The alloy is used in aerospace applications. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as joining. Filing Code: AL-371. Producer or source: Alcoa Mill Products Inc.
This content is only available as a PDF.