Abstract

Anviloy 1150 is tungsten-bearing sintered alloy of high density and high strength. It is a PM product and one of a series of alloys with densities 50% greater than that of lead. Anviloy 1150 is a material developed specifically for its high-temperature strength and excellent thermal conductivity. It is used to best advantage in place of lower-conductivity, high-temperature tool steels. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as machining and joining. Filing Code: W-16. Producer or source: CMW Inc. Originally published February 1970, revised November 2000.