Abstract

J and L 2205 is a ferritic-austenitic duplex stainless steel. It resists stress-corrosion cracking very well and has good pitting and general corrosion resistance. Its high strength and stress-corrosion resisting characteristics are a reflection of its duplex microstructure. Its uses include pipe, tubing, tanks, and heat exchangers for the chemical industries. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-773. Producer or source: J & L Specialty Steel Inc.