Abstract

Uddeholm tooling AISI 01 is general-purpose, oil-hardening tool steel suitable for cutting, shearing, and forming. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on heat treating, machining, and joining. Filing Code: TS-568. Producer or source: Uddeholm Corporation.