Abstract

Sandvik SANBAR 61 is a high-strength silicon steel with good toughness and impact resistance in the as-rolled condition. The primary application is tapered rods. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on forming, heat treating, and machining. Filing Code: SA-502. Producer or source: Sandvik.