KHR35C Hi Si is similar to Kubota alloy KHR35C but with added silicon levels to improve carburization resistance. The typical application is ethylene furnace tubing. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance as well as casting and joining. Filing Code: SS-755. Producer or source: Kubota Metal Corporation.