Sumitomo weldable seamless 13Cr-M is a corrosion-resistant oil country tubular goods line pipe product that resists wet hydrocarbon products containing carbon dioxide. Increased weldability is developed by modifying the chemistry to ultralow carbon content. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on low and high temperature performance, and corrosion resistance as well as joining. Filing Code: SS-752. Producer or source: Sumitomo Metal Industries Ltd.