Abstract

Olin alloy 186 provides high thermal stability for elevated-temperature connector applications. This alloy provides exceptional resistance to loss in contact because of its excellent resistance to stress relaxation. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on forming. Filing Code: CU-635. Producer or source: Olin Brass.