Abstract

Kubota alloy KHR12C is an austenitic Fe-Cr-Ni-Nb casting alloy developed from the well known HH type II grade. This alloy is superior to other grades in components that are subjected to frequent thermal cycling and shock. The alloy is available in both centrifugal and static castings. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance as well as casting and joining. Filing Code: SS-738. Producer or source: Kubota Metal Corporation.