Crucible 154 CM is a hardenable chromium stainless steel with molybdenum to improve hot hardness and corrosion resistance. Typical applications include bushings and bearings where high hardness is needed. This datasheet provides information on composition, physical properties, and hardness. It also includes information on forming, heat treating, machining, and joining. Filing Code: SS-737. Producer or source: Crucible Service Centers.