Mi-Tech high-density (HD) metals are high-strength, machinable, tungsten-base materials used where high density and strength are required. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on machining and joining. Filing Code: W-20. Producer or source: Mi-Tech Metals Inc.