Abstract

KHR 35CT HiSi is a modification of KHR 35C HiSi (see Alloy Digest SS-753, July 1999, and SS-755, August 1999) by the addition of both silicon and titanium as the microalloying additions. The strength, oxidation resistance, and metal dusting resistance improve its use for ethylene pyrolysis coils. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on casting. Filing Code: SS-767. Producer or source: Kubota Metal Corporation.