Abstract

WRM alloy 5248 is a phosphor bronze alloy with higher strength and better stress relaxation resistance than 10% tin alloys. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and bend strength. Filing Code: CU-640. Producer or source: Waterbury Rolling Mills Inc.