WRM Alloy C15500 is a copper alloy with one of the best combinations of electrical, mechanical, and relaxation properties. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: CU-616. Producer or source: Waterbury Rolling Mills Inc. Originally published May 1998, corrected October 1999.