Abstract

Olin 175 has a relatively low beryllium content and a moderately high electrical conductivity. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming and heat treating. Filing Code: CU-622. Producer or source: Olin Brass.