Abstract

INCO-CORED 82DH (down-hand) and 82AP (all-position) flux cored wired were developed as companion welding materials to INCONEL Filler Metal 82 and INCO-WELD A Welding Electrode. Applications include welding Inconel or Incoloy alloys to themselves or to ferritic, austenitic, or ferric/austenitic duplex stainless steels. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on joining. Filing Code: Ni-543. Producer or source: Inco Alloys International Inc.