Abstract
Allloy AC 66 is a high temperature austenitic steel with alloying additions to improve oxidation resistance and alloying limitations to improve internal oxidation. Typical applications are waste handling to energy boilers and coal gasification plants. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-710. Producer or source: European metal producers.
This content is only available as a PDF.
Copyright © ASM International® 1998
1998
ASM International
Topics
Austenitic stainless steel
Waste handling and recycling
Corrosion-resistant alloys
High-temperature alloys
Chemical composition
Oxidation resistance
Heat treatability
Joinability
Machinability
Workability
Creep properties
Elastic modulus
Tensile properties
Physical properties
Thermal properties
You do not currently have access to this content.