VANADIS 60 is a high-speed steel with an addition of cobalt. The alloy is particularly suitable for cold-work tooling where highest wear resistance and highest compressive strength are required at the same time. This datasheet provides information on composition, physical properties, and hardness. It also includes information on high temperature performance as well as forming and heat treating. Filing Code: TS-565. Producer or source: Uddeholm Tooling AB.