Abstract

MO-RE 40MA is a fully austenitic heat-resistant alloy for elevated temperature applications. The alloy is microalloyed for creep strength and oxidation resistance. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance. Filing Code: Ni-548. Producer or source: Duraloy Technologies Inc.