Abstract

Colmonoy 805 is a nickel-chromium-boron alloy with coarse particles of chromium boride added to give it excellent sliding-type abrasion resistance. The alloy contains chromium boride in the matrix as large added particles. It is supplied only as a crushed powder for application with Colmonoy’s Fuseweld process. This datasheet provides information on composition, physical properties, microstructure, and elasticity. It also includes information on corrosion resistance as well as joining and powder metal forms.Filing Code: Ni-233. Producer or source: Wall Colmonoy Corporation. Originally published September 1976, revised December 1998.