MO-RE 10 is a fully austenitic, heat-resistant cast alloy with good creep-rupture properties. Typical applications include pyrolysis and reformer tubing. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance as well as casting. Filing Code: SS-731. Producer or source: Duraloy Technologies Inc.