Abstract

Tristelle Alloy 5183 is a stainless steel-base hardfacing alloy designed to replace the traditional cobalt alloys for use in nuclear-plant applications. This datasheet provides information on composition, and physical properties as well as fracture toughness. It also includes information on corrosion and wear resistance as well as joining. Filing Code: SS-688. Producer or source: Stoody Deloro Stellite Inc.