Abstract
Nitro-Die is a tough nickel-chromium-molybdenum-vanadium-nitrogen alloy with good high-temperature physical properties. The alloy is enhanced with micro-additions. This datasheet provides information on composition and hardness. It also includes information on heat treating and machining. Filing Code: TS-556. Producer or source: A. Finkl & Sons Company.
This content is only available as a PDF.
Copyright © ASM International® 1997