Abstract

Sandvik 3R64 is an austenitic stainless steel with a high molybdenum content. Significant properties are improved general and pitting corrosion resistance in comparison with Type 316L. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as heat treating and joining. Filing Code: SS-686. Producer or source: Sandvik.