Abstract
Conicro 5010W has a face-centered cubic structure and is a cobalt-base alloy containing chromium, tungsten, and nickel. The alloy is used in aerospace applications and in the heat-treatment industry. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on forming, heat treating, machining, and joining. Filing Code: CO-103. Producer or source: VDM Technologies Corporation.