HPM Evanohm S is a nickel-base alloy having low-temperature coefficient of resistance and high electrical resistivity. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on heat treating. Filing Code: Ni-526. Producer or source: Hamilton Precision Metals Inc.