Nicrobraz is a free-flowing nickel brazing filler metal with a wide melting range and low diffusion with most base metals. The brazing metal meets AWS, AMS, G.E., and other specifications. This datasheet provides information on composition, physical properties, and hardness. It also includes information on corrosion resistance as well as joining. Filing Code: Ni-525. Producer or source: Wall Colmonoy Corporation.