Abstract
3M TITANIUM MATRIX COMPOSITES are produced by electron-beam evaporation to apply Ti-6Al-4V coating to high-strength, high-modulus silicon carbon fibers. The resulting composite has increased strength and stiffness over monolithic titanium/titanium alloy parts. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive and shear strength as well as creep and fatigue. It also includes information on surface treatment. Filing Code: TI-111. Producer or source: 3M Metal Matrix Composites Program.
This content is only available as a PDF.
Copyright © ASM International® 1997
1997
ASM International
You do not currently have access to this content.