Abstract
Vasco 9-4-30 (0.30 wt% C) is a premium quality aircraft steel which combines high tensile strength with good fracture toughness. It is a heat treatable alloy capable of developing ultimate tensile strengths greater than 250 ksi. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness. It also includes information on high temperature performance as well as heat treating, machining, and joining. Filing Code: SA-491. Producer or source: Vasco, An Allegheny Teledyne Company.