Abstract
Lanxide 92-X-2050 is an aluminum-10 Silicon-1 Magnesium-1 Iron alloy with 30 vol.% of silicon carbide particulate. This metal-matrix composite is designed to outperform the unreinforced counterpart. The alloy-matrix composite is available as die castings. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also includes information on casting. Filing Code: AL-343. Producer or source: Lanxide Corporation.